  • How delicate is powder - before baking?

    I'm wondering about how delicate the powder coated part will be after it has the powder applied and I am transferring it to the oven - I have about 30-40 feet from where I would apply powder to where the oven will be located. The floor is slightly bumpy in places and I'm wondering if I need to carefully hand carry the parts or could I wheel them? What about drafts?

    Thanks for your help.

  • #2
    Re: How delicate is powder - before baking?

    You could safely wheel the part over. If maintains a pretty good static charge, which keeps the paint applied to the part.

    Breezes should be no problem.
    --
    Mike Caswell
    Caswell Inc
    http://www.caswellplating.com