  • johnny933
    replied
    Guess i'll try to get it out one more time. Hopefully i'll have some luck.

    Leave a comment:


  • drfjr1976
    replied
    I have done a few with them. I usually remove them because they are held in with a seal that may melt during the curing process.

    Leave a comment:


  • johnny933
    started a topic Coating part with glass piece

    Coating part with glass piece

    I want to coat an alum. clutch cover off an atv. Here's the problem. Theres a small glass eye that I cant figure out how to get out. will it break during heating? Have any of you guys done this with the glass view finder for the oil not removed?