Announcement
Collapse
No announcement yet.
Coils and Leafs
Collapse
X
-
Most coils come from the factory powdercoated, at least most aftermarket springs do.
Just do a normal cure and you'll be alright.
Leave a comment:
-
Coils and Leafs
I think I saw something about this but cant find it.
Here's the thing......I got someone who wants there coils(on car) coated and was wondering if it affects the spring during cooking. Does it weaken it any? I've seen them done, but dont want to ruin someone's part in the long run. Please help.Tags: None
Leave a comment: