    Sounds ok to me. We do multiple parts in the oven and have no problem.

    Leave a comment:


  • j-mcguigan
    started a topic Curing multiple parts?

    Curing multiple parts?

    Can multiple parts be cured at the same time in the same oven. Like if the heat and cure times are the same for both, you wouldnt have to have 30 different bake cycles for 30 little parts,right?