    When applying clear, do I put the clear on when the part is fresh out of the oven? Can I wait untill the next day, and do it then? How thick should it be? Any help and any other pointers would be great.

    Thanks,
    Kris

  • #2
    I always have trouble judging how much i am spraying on it when the part is still hot. The clear flows out imediately and looks like it was dry shot. I recomend spraying the clear when part has cooled down and it should look like if you sprayed any other powder.