Anyone have or know somewhere where I can find out which blast media is best to use on certain metals? I'm just starting out and have no clue what to use on what and what not to use.
Announcement
Collapse
No announcement yet.
Blast Media info
Collapse
X
-
I use "Black Magnum" available at almost any Menards. It's relatively cheap, safer than silica sand, and works on most steel and aluminum parts. I usually pay about $5 for a 50# bag. I know some of the guys pay less than that, but for a hobbyist that's not too bad. You can probably get it cheaper if you buy quantity.
Hemi-T
Comment
-
Menards must be a ^ North thing. I've never heard or seen of them. And cant find any black magnum any where. Although there is a place here in SC that makes blasting material called Black Diamond but you have to call one place then they ship the sand, coal or what ever they use to another like 30 mins away from where i live and that guy cooks it and makes it.