  • Can I powder coat polished aluminum?

    If I polish aluminum, can I use clear PC to protect it from oxidization?

  • #2
    Yes it works nicely for that.

    Comment


    • #3
      what about the chemicals used to polish the aluminum. wouldnt there be bubbles on the clear coat This is something I am interested in doing, becase my bike frame is polished and its just a hassle to keep polished all the time

      Archer
      I Plead the Fifth!

      Comment


      • #4
        you can clear polished but when i did it it came out a milky color .... but besure to clean the part good to remove all the compounds .. i use hot soap and water to clean after polishing

        Comment