Guest repliedyou can clear polished but when i did it it came out a milky color .... but besure to clean the part good to remove all the compounds .. i use hot soap and water to clean after polishing
-
what about the chemicals used to polish the aluminum. wouldnt there be bubbles on the clear coatThis is something I am interested in doing, becase my bike frame is polished and its just a hassle to keep polished all the time
Archer
Leave a comment:
-
Can I powder coat polished aluminum?
If I polish aluminum, can I use clear PC to protect it from oxidization?Tags: None
Leave a comment: