Announcement

Collapse
No announcement yet.

air comsumption

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • jung4g
    replied
    Honestly, if you've got any air consumption worries about powder coating, they are wrongly placed. The only reason to have a little more air is for a compressed air blower to clean the gun between colors.. the nitrogen tank is a great idea.

    Leave a comment:


  • y2khardtop
    replied
    My eastwood gun uses hardly any air at all. I actually am running off of a Nitrogen tank, that way I can skip the water filter.

    My gun only uses 6-10psi, so the air-flow is quite low. It even says you can use a portable air pig!

    Leave a comment:


  • sam4
    started a topic air comsumption

    air comsumption

    Hi,
    Can someone told me what is the average consumption of a PC gun with a fluidized bed (1 ft2)?
    Is the tank size important for running only a PC gun?

    many thanks
Working...
X