    I've never used the other two deflectors that came with my gun, the one that was on it ( the med size) and it has worked for everything great so far, what would the advantage be of the large one and the small one?
    Pro-Tech Powder Coating
    93976 Ocean Way
    541-247-8168
    [email protected]
    Gold Beach,Oregon

  • #2
    Ya know, i was wondering the same thing. Guess I should do more reading. hmmm.
    I Plead the Fifth!

    Comment


    • #3
      To get into tight corner's and deep cavitie's I actully take the
      deflector off all together
      Art
      Art in Peterborough

      Comment


      • #4
        have to give that a try Art..tanks for da tip...