    just read an add for parts for a 41 willys coup and it said it the window frames were cromed over fiberglass...anyone know how this done? cant be pc..or maybe it could i dont know..
    Pro-Tech Powder Coating
    93976 Ocean Way
    541-247-8168
    [email protected]
    Gold Beach,Oregon

  • #2
    Maybe chrome strips attached to fiberglass? You can use a conductive coating to get the powder to stick, but need to cure at a lower temp for a longer period of time. It's a very tricky process but it can be done. The conductive coating can also be used for chroming.

    Comment


    • #3
      could you please point me in a direction i might learn more PLEAZZZZZe..
      this interests me,,,and im not at all sure where to start looking..
      Thanks
      Wayne
      Pro-Tech Powder Coating
      93976 Ocean Way
      541-247-8168
      [email protected]
      Gold Beach,Oregon

      Comment


      • #4
        Wayne if you e-mail me a copy of the add I probably can tell you how they do it.