    The compression side of a turbo does not get anywhere near as hot as the Turbine/exhaust side. Does it stay cool enough that I could powder coat it?

    Per a email from Caswell: About 350 deg F sustained temperature.


    WOOT!!!! I Hate this support I get on this board and the company. Ruins me for all those other companies that suck at both support and customer service :P

  • #2
    i have seen afew sets of cold sides done in power coat and look good with out problems to them.
    D.I.L.U.S.I.

    Drive It Like You Stole It

    Comment


    • #3


      here is a pic on a turbo charger that i got from a member says he put 8k miles on it and nothing is wrong with the finish so far...

      hope this help bro good luck..
      D.I.L.U.S.I.

      Drive It Like You Stole It

      Comment


      • #4
        sweet...thanks a lot