    i got about 5 lb's of metal flake from when i was painting car's the old school style .. i did not even know i had them can i mix them in clear powder and shot them ..just as you would when spraying a car

  • #2
    Now that would be worth a try. I would at least do a sample piece. Keep us informed on this.

    Comment


    • #3
      The illusion powders make a nice metal flake.They come in different colors and are very nice. I add 1 teaspoon of illusion the a cup of clear, gives just a hint of flake without changing the base color. 50/50 mix is very heavy metallic look. Try it.

      Comment


      • #4
        i will try it .. and post a pic ... Stay Tune!!!!!

        Comment


        • #5
          hey post some pics when u do this. i hope it comes out nice
          D.I.L.U.S.I.

          Drive It Like You Stole It

          Comment


          • #6
            hey did you try the flake yet?
            D.I.L.U.S.I.

            Drive It Like You Stole It

            Comment


            • #7
              i will get to it this week i hope .. every time i get a chance to do something for myself.. i end up doing something for some one else or the fire siren go's off or the kid need's to go some where 7more years and she can take her own self... i will post a pic when i get it done

              Comment


              • #8
                i here ya on that. well just wanted to know i will keep an eye open for your work. thanks for the fast response
                D.I.L.U.S.I.

                Drive It Like You Stole It

                Comment


                • #9
                  i here ya on that. well just wanted to know i will keep an eye open for your work. thanks for the fast response
                  D.I.L.U.S.I.

                  Drive It Like You Stole It

                  Comment


                  • #10
                    What was the results with the metal flake?

                    Comment


                    • #11
                      heard thru the grape vine that most metal flakes are actually ground polyester...dont know this for sure but one of the tackle paint suppliers I use to buy from said that...just a thought...