Having a real dust problem in my shop.You can actually see the dust in the air being attracted to the part while spraying.Any great solutions out there for this problem?Oh and one more thing.NEVER try spraying alittle more powder on a part while curing thinking it will melt and blend in.It absolutely will not and you will be doing some stripping.