Announcement
Collapse
No announcement yet.
Mr. Heater
Collapse
X
-
Guest repliedit is an ir heater
-
Guest repliedi use propane i converted a bbq
Leave a comment:
-
The real fine powder floating in the air, is what's highly flammable. I also use a Mr. heater for very large items.
Leave a comment:
-
My oven is built out of angle iron, and cement board and measures 6ft wide, 3 feet deep and 6 feet high. For heating I have used for over 2 years 4 triple Mr Heater infrared elements with great success. The next oven I will use sheetmetal and have it well insulated, but this has worked great for me for 2 years.
Leave a comment:
-
Mr. Heater
I'm new to this so some of it is confusing, If the powder is flammable before curing how can a Mr. Heater be used to cure. Thanks in advance, RonNTags: None
Leave a comment: