    Does anyone have experience painting over powder coated products? I have iron stair parts that have a black powder coating on them. I need to know what kind of paint can be used and what is the application process?

    Your help would be appreciated.

  • #2
    your best bet is to sand blast them and paint them with an epoxy paint

    Comment


    • #3
      the powders tuff..i would probably just light sand and paint over it all with a good epoxy paint.,,,do a test strip in an out of the way place to be safe though..myself I havent had any probs....this is good...I was at a big full blown pc company last week..I watched a guy in there QC area carring around a hand full of magic makers..and every now and the ...dotting the eye ..

      Wayne
      Pro-Tech Powder Coating
      93976 Ocean Way
      541-247-8168
      [email protected]
      Gold Beach,Oregon

      Comment

      Working...
      X
      😀
      🥰
      🤢
      😎
      😡
      👍
      👎