  • jtagger19
    replied
    sounds like it was still hot when you took the tape off
    and 450 is way to much , I cure at 380

    Leave a comment:


  • wolf13
    started a topic PC is rubbery

    PC is rubbery

    Hello all,
    I PC'd some engine cases in a wrinkle black finish, and as I pulled off the tape, the coating is rubbery. Is this normal or was my cure time too short? Time was about 20 min @ 450f.
    Thanks,
    Wolf