Originally posted by customandsound
Announcement
Collapse
No announcement yet.
Tech Line Coating, will this gun work?
Collapse
X
-
-
Guest repliedthat look's good ... noob you can bake it at 700f for an hour and it will be fully cured ....
Leave a comment:
-
Well IT WORKS!!! I Coated the Heads on my motor and I think they came out great. Now, wait 5 days for full cure. I used Satin Black and it is a lot glossier then I expected. Looks good with the aluminum block and Black waterpump. Can't wait till I PC the rest of the parts on the motor. I will post Pic's in the album as soon as I get them off the camera.
Edit to add Image and let you know that I post Pic's in the Album
Leave a comment:
-
Well I picked up the gun this weekend and depending on what happens this weekend I might be doing my exhaust manifolds. that is if I get all the mock up done with my brackets!
Leave a comment:
-
Originally posted by customandsoundwith over 200 emails a day i get confussed .. can you resent it and put noob in the subject line.... sorry about that ...Thanks look forward to getting pic's. Also if you need parts let me know, I have about 1/2 of a one in the shed :P
Leave a comment:
-
Guest repliedwith over 200 emails a day i get confussed .. can you resent it and put noob in the subject line.... sorry about that ...
Leave a comment:
-
Hey, I sent you an email for the links and pics of that big block fiero but it seens that you blew me off!!Thats ok, I will find you!!!!
nelvar42 email is the addy.
Leave a comment:
-
Guest repliednope i want to make a jet boati got 2 of them one i am tossing a kit car body on and the other is going to be all out strip.. i hauled this one up from my uncles in rockingham nc and i need to haul up the other one in week or so
randy email me and i will give you a link to the pic's i took when it was bad here... sorry noob for stealing the topic
Leave a comment:
-
are you puting a big block in it so it doesnt float away if you get another storm:P
Leave a comment:
-
Guest repliednoob email me i will send you some pics of a sick looking car like yours i have in my yard... we are about to drop a big block in it
[email protected]
Leave a comment:
-
Guest repliedi don't see why it would not work ... i use a detail gun when i spray my part's.... i got an old brinks i was going to use it for the big parts ... but i think it will work fine
Leave a comment:
-
Tech Line Coating, will this gun work?
I am looking at getting a sprayer just for my techline coatings, will this one work?
http://www.harborfreight.com/cpi/cta...emnumber=43762Tags: None
Leave a comment: