Powder Coating over anodizing?
Collapse
X
-
I had good luck coating over anodize. Just make sure you wipe it down just like any other part you were going to coat.
-
Powder Coating over anodizing?
Hey all:
has anyone tried powder coating over an item that has been previously anodized? If so, what were the results? Also did you do any special prep or prestripping of prebaking?
Thanks
BobTags: None