  • Guest's Avatar
    Guest replied
    yep it only takes a few sec's to strip it .... you are looking at more problems than it is worth .... just like dale said

    Leave a comment:


  • johnny933
    replied
    I gotta say Dale is 100% correct. You can do it but you should just start over.

    Leave a comment:


  • DALE
    replied
    By doing this you are now up to a third or fourth coat.Can it be done--yes.
    Should it be done--no, strip it,start over and do it right. The more coats you add the more difficult it becomes. Also once you exceed a certain thickness you begin taking the durability lower instead of higher.

    Leave a comment:


  • Robb
    started a topic re-shoot a color over a clear?

    re-shoot a color over a clear?

    can i re shoot a metallic color over a clear? I don't like the first results of the metallic and clear coat.