    ok.....got my hi-temp powder from caswell (btw I was impressed with the speed it got to the west coast in) I read thru the past threads about doing headers...my question is what is the best cooking temp, i read 500f somewhere....I havent messed with this stuff befor and seeings how its sorta spendy want to get it right the first time.
    Pro-Tech Powder Coating
    93976 Ocean Way
    541-247-8168
    [email protected]
    Gold Beach,Oregon

  • #2
    I use a min. of 500F and bake about 10 extra minutes. If they are for me after install, I run the motor in short cycles to season the coating a bit more.

    Comment


    • #3
      Thanks Dale....was gonna call and talk at ya but ive been up to my tail in aligators and im supposed to be draing the swamp...talk at ya laterzz...

      Wayne
      Pro-Tech Powder Coating
      93976 Ocean Way
      541-247-8168
      [email protected]
      Gold Beach,Oregon