Rigid Board Insulation for Oven Construction??

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • Rigid Board Insulation for Oven Construction??

    Hey All:
    I've seen some of you talk about "rigid board" insulation. I have been trying to find a source to purchase from. I looked at Home depot & othe rlocal lumber yards, no go. I would like a 4'x8'x2" panel that is rated for 850F.
    I am in the process of building a 20'D x 8'W x 8'H oven from a metal storage container (Mini warehouse). I plan to glue the panels to the outside using a high temp adhesive with a caulking gun.
    Any help would be greatly appreciated.
    Bob
    www.capecodpowdercoating.com

  • #2
    850 F? why so hot??

    Comment


    • #3
      850 F? why so hot??
      if for the same reason than me , better safe than sorry

      I used in mine a stuff called knauf it's 4'x8'x2" it holding great at 700 for ceramic coatings

      Comment


      • #4
        Re: Rigid Insulation panels

        Thanks Jtagger:
        Can you tell me where I can buy it?
        Bob
        www.capecodpowdercoating.com
        www.capecodpowdercoating.com