Announcement

Collapse
No announcement yet.

Looking for this color...

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • Looking for this color...

    Anyone know a color as close tothis as possible?

    http://store1.yimg.com/I/hopup1_1821_107201220
    WEIRD Performance & Coatings
    Sweden

  • #2
    Looks very familiar to chrome smoke to me

    Comment


    • #3
      im pretty sure I saw a color sim to that in tiger dry book, when I get to the shop this morning I will try and find the number for you...with tiger you will have to buy 5pound min and they tend to be on the spendy side...
      Pro-Tech Powder Coating
      93976 Ocean Way
      541-247-8168
      [email protected]
      Gold Beach,Oregon

      Comment


      • #4
        Originally posted by Blademan
        im pretty sure I saw a color sim to that in tiger dry book, when I get to the shop this morning I will try and find the number for you...with tiger you will have to buy 5pound min and they tend to be on the spendy side...
        Thanks, since i live in Sweden i think ill have to fund another supplier here, but information on the color would be helpful.
        WEIRD Performance & Coatings
        Sweden

        Comment


        • #5
          went thru all my color charts, even looked at the wheel in adobe photo shop and to be honest its really hard to tell for sure the actual color, it appears to be two different colors depending on which monitor im useing, but my guess is looking at some things ive shot with black chrome is its black chrome, now im on a quest..going to go down to the tire shop and grab a bunch of there rim charts to see if i can find out for sure..all n all I think the black chrome will be real close..
          Pro-Tech Powder Coating
          93976 Ocean Way
          541-247-8168
          [email protected]
          Gold Beach,Oregon

          Comment


          • #6
            Looked at Caswells limited gold, seems close but hard to determine by their webpage, anyone got any image of something coated with Limited Gold?
            WEIRD Performance & Coatings
            Sweden

            Comment


            • #7
              I used chrome smoke and it does look like that.
              WARCHILD

              Comment

              Working...
              X