  • Gun trouble... again

    OK.. I have the Harbor freight gun unit, and the powder dosent seem to flo evenly, the powder flo will start out good then get thin.. and then i give it a little shake.. and its ok for a few seconds and then it starts to thin out again.... I cleaned the hell out of it the other day with no effect, does the same thing.
    Any ideas?
    If it jams; Force it. And if it breaks it needed replacing anyway.

    I can go from 0 to "What seems to be the problem Officer?" in 3 seconds."

  • #2
    use it at 20PSI
    and coat with small circular motions that will get you an even coat
    most of all practice and get to know the gun.