I've done TGIC transparent gold over chrome powder and I didn't like it
I looks like a very light yellow
It looks a lot better over chrome or polished aluminum
but then again not many people are willing to chrome or polish and then powder coat gold over it cuz it's way to expencive
again this was a different gold than caswells .
Announcement
Collapse
No announcement yet.
gold color?
Collapse
X
-
gold color?
i was wondering how well your gold metalic hybrid color would work for dirtbike hubs (the inside part of the wheel where the spokes go and axle goes through). and is there anything different i need to do because it is a hybrid powder? or does anyone know of another gold color powder? thanks for any replyTags: None