Well I guess they are calling the Old 525 Super Chrome now, if you look at the color chart thats my Valve cover and I used 525. Applies the same as the rest but you need to clear coat it if used outside..Jim Shuster
www.backyardpowdercoating.com Sold.....
www.chrissys68mustang.com Hobbie
www.photogserver.net Web Hosting.
-
Re: Supr Chrome powder
I used it, worked well, but like Jiim mentioned it needs to be clear coated over (if used near UV / sun). Once you clear coat, it does dull some of the shine, but still looks good, for sure not as deep & rich as real chrome!
Happy New year
Bob
www.capecodpowdercoating.com