    when doing a candy color over chrome, the candy color wasnt thick enough so you can see some chrome through it, can i just do another coat of the candy red or do i have to strip it and start over? thanks randy...

  • #2
    if you fully cured the second coat (candy color) you will not get a good adhesion on a third coat ( second candy) wich can cause future problems
    but still you can do it
    pre heat it to 150 and recoat.