I let it cool to about 150- 160 F. If you let it stay much higher than that the powder starts to melt while you are spraying it and makes it hard to judge how much you are putting on.
Leowww.tinmans.net
"Life is not a journey to the grave with the intention of arriving safely in a pretty and well preserved body, but rather to skid in broadside, thoroughly used up, totally worn out, and loudly proclaiming -- WOW--What a Ride!!!" ----- Unknown
Comment
-
everything noob said, and I wipe down the part just befor coating with acetone..