What powdertype is best suited for coilsprings for cars?
Announcement
Collapse
No announcement yet.
Powdertype for coilsprings?
Collapse
X
-
Tags: None
-
Re: Powder coat for Coil Springs
Hey Zpider:
I have done a couple of sets of coils. I used glass balck on some & flat black on others. I even have done the same on snow plow trip springs. None have come back with complaints.
Bob
-
Did you use Polyeurethane or Polyester powders? Just want to know which is more flexible.WEIRD Performance & Coatings