    the exhaust is 1200 so the boot's will be good up to 700 in an oven . but that is a good find!!!!

    Leave a comment:


  • buzzurd
    started a topic weekend discovery

    weekend discovery

    I needed a weird size high temp plug this weekend which I did not have.Did alittle experiment and found that spark plug boots will withstand 400 degrees for 30 min.Saved my butt and possibly someone elses.Just thought it may be worth mentioning.