  • jtagger19
    replied
    I get things steel shot at a local machine shop and haven't had any problems so far.

    Leave a comment:


  • kchotboat
    replied
    If you leave the old powder on I would use steel wool or 220 sand paper.

    Leave a comment:


  • Blademan
    replied
    yes you can coat over the old pc but not recommended...., I would suggest you strip the item and recoat. as far as the steel shot I cant say cause Ive never used it.

    Leave a comment:


  • showroomexpress
    started a topic to strip or not to strip?

    to strip or not to strip?

    #1 Can you powder coat over exsisting powder coat without stripping off the old powder ? The new powder is a different color than the base coat. #2 If the old powder does have to be stripped first ,will steel shot damage the base metal aluminum? Thanks in advance.............John