poweder coat over real chrome
Collapse
X
-
-
Originally posted by MaxxxDid you preheat or have any trouble with outgassing?believe it or not. hung it up, dusted it and baked. Going to do the same process this weekend on a set CAI tubes.
Leave a comment:
-
I have PC'd over chrome before with great results. I did not use a Clear/Transparent color. I used Safety yellow and it has held up great.
Leave a comment:
-
poweder coat over real chrome
I tried searching for an answer to this, but couldn't find anything. Has anyone tried to put a transparent (or clear) powdercoat over an aluminum piece that already has a real chrome finish? I would imagine that the chrome would handle the heat, but I'm worried about outgassing and discoloration. I'm looking at buying a brand new aluminum license plate frame with a new chrome finish, then putting a liquid smoke powdercoat over it. Anyone eveer try this?
Thanks!Tags: None
Leave a comment: