  • Guest's Avatar
    Guest replied
    noob for get it i POLISHED it instead

    Leave a comment:


  • Guest's Avatar
    Guest replied
    i just did a 7 angle valve job on my head i had it all bolted up then i was going to coat it .. but i ended up taking it off any how .. i think that was you that called today .. sorry i missed ya!!

    Leave a comment:


  • Noob2PC
    replied
    Re: noobpc2 i need to know

    Originally posted by customandsound
    when you did the head on you motor was it whole or just the shell?
    You mean the Ceramic Coating? I left it on the Motor, the sleeves are a PITA if they slip and I did not want to affect the compression since they were all 170+. I just taped off the entire motor and sprayed the head. I should be doing the Exhaust Manifolds and Exhaust system today. Will Post Pics when that is done.

    Leave a comment: