    i'm sure this is possible, but i figured i would ask. I would like to do 3 different colors plus clear on a set of valve covers. Emblem one color, Lettering another, then cover in aluminum pc. then clear the whole package. if this is possible, any and all recomendations are welcomed.

    thanks, Dave
    Never argue with an idiot...they will bring you down to their level and beat you with experience.

  • #2
    Well here is 2 colors, so I'm sure 3 can be done. Just watch your cure times. Or if you can do 2 colors at the same time...
    This was Chrome, Lolli Pop Blue and clear..
    Jim S...
    Jim Shuster
    www.backyardpowdercoating.com Sold.....
    www.chrissys68mustang.com Hobbie