    Guest replied
    no.. to both .... i have a part melt and deform

    Leave a comment:


  • warchild
    started a topic Pewter be powder coated?

    Pewter be powder coated?

    Can Pewter be powder coated? I know nothing of this type of metal. Will it melt at 400? And I would think it would need to be preheated too.