Despite all of my efforts, I cannot find any sites where someone has at least tried to PC an entire auto body. I see where BMW is using a low cure PC clear coat, but that's it.
This is a restored 1967 off-road vehicle;
I'm not looking for a show-quality finish. Durability is more important than wax-ability.
The body is sans paint and anything other than metal.
I have plenty of plaques.
It would actually be cheaper than a 2-part urethane liquid paint.
I'm not too worried about warpage because the steel is well supported.
I have removed all of the rust and there is no filler on it.
Any filling will be done with Lab Metal.
Any links, suggestions, thoughts, money....would be appreciated.
Thanks,
Brog
Here is a link of the color that I am going for.....Mustard
This is a restored 1967 off-road vehicle;
I'm not looking for a show-quality finish. Durability is more important than wax-ability.
The body is sans paint and anything other than metal.
I have plenty of plaques.
It would actually be cheaper than a 2-part urethane liquid paint.
I'm not too worried about warpage because the steel is well supported.
I have removed all of the rust and there is no filler on it.
Any filling will be done with Lab Metal.
Any links, suggestions, thoughts, money....would be appreciated.
Thanks,
Brog
Here is a link of the color that I am going for.....Mustard