    Just wondering if there would be a demand for stencils for PC'in.Possibly flames or tribal art or even custom designs.Could maybe be made available through Caswell if they were interested.
    I currently have thousands of designs for motorcycle tank and fender sets,automotive and commercial applications. Thanks for any input Steve

  • #2
    I might be interested in trying a couple. Are they hi-temp stencils?

    Comment


    • #3
      You can buy the large sheets of the hi temp green tape and have them cut out on the the same machine that makes decals. I have been looking for a used one.

      Comment


      • #4
        Originally posted by kchotboat
        You can buy the large sheets of the hi temp green tape and have them cut out on the the same machine that makes decals. I have been looking for a used one.
        I have a 24" plotter for cutting vinyl. Where do I find the sheets of tape??

        Comment


        • #5
          i have the address at work if you email me later I will send it to you
          Pro-Tech Powder Coating
          93976 Ocean Way
          541-247-8168
          [email protected]
          Gold Beach,Oregon

          Comment


          • #6
            I've been looking for a way to pc some color on a wine bottle after etching. Do you leave the stencil on while it bakes or how does this work? I have a client that wants roses or grape vines on her bottles. Have anything that might work?
            Thanks,
            Don

            Comment


            • #7
              Originally posted by remotestartdepot
              Originally posted by kchotboat
              You can buy the large sheets of the hi temp green tape and have them cut out on the the same machine that makes decals. I have been looking for a used one.
              I have a 24" plotter for cutting vinyl. Where do I find the sheets of tape??
              I will ask a friend of mine who has a full time pc shop. I saw those a couple of weeks ago at his place.