    has anyone had any luck wet sanding out or buffing out orange peel or a high spot? if you have please tell me what you used.. thanks randy

  • #2
    I have sanded and then repowder coated a few of my own stuff to see how it holds up.

    Comment


    • #3
      randy,
      I have wetsanded some parts that were o p'ed. I used 1500 wet sand then hit it with a light compound and then a polish and it came out some as glass.

      Comment


      • #4
        i wet sanded and polished .. just as stated above perfect did not even know what happen