sanding parts smooth
Collapse
X
-
The only time I sand or grind is when there is spatter, an ugly weld, or flashing from casting. Otherwise I just blast it and go.
Leave a comment:
-
You just need to sandblast the part. If I am trying to take casting marks out of a part I will sand them down and then sandblast.
Leave a comment:
-
re: sanding parts smooth
If the item is just been sandblasted, you will not need to sand it.
Good Luck
Bob
Leave a comment:
-
sanding parts smooth
to prep a piece of metal befor pc what do u sand or ground down the piece with thanks or do u have to if u already sand blasted itTags: None
Leave a comment: