  • Guest's Avatar
    Guest replied
    i spray right over it .. clean it real good !!!

    Leave a comment:


  • seanc
    replied
    I've been PCing zinc palted parts quite successfully. Zinc is a great base for PC. Some pictures:

    http://www.hogheaven.com/hobby/plati...tes/index.html

    If the zinc parts have a chromate conversion coat, simply cleaning them good should be enough. Chromate coversions are a good base for PC.

    If the parts are raw zinc, pre-etch them for about 10-20 seconds in a 3-5% muriatic acid pickle. This will remove surface oxidation & activate the zinc surface.

    Sean

    Leave a comment:


  • pdeinc
    replied
    Whether you get all the zinc off or not is pretty much immaterial. It's a metal, not much different than any of the fillers used to prep parts with. More important is that it's clean.

    Leave a comment:


  • CaptainChauncy
    replied
    I just blast off the zinc coating and then treat it like a normal part. It probably wouldnt hurt to prebake it though. Ive only powdercoated a couple small parts that previously had a zinc plating but they came out great

    Leave a comment:


  • trsick
    started a topic Powder of Zinc plating.

    Powder of Zinc plating.

    Hey All:
    I have a customer that wants my to PC on items that had been previously zinc plated. Do I need to do any special prep? Or do I need to blast off the zinc coating first
    Thanks
    Bob