  • warchild
    replied
    I to do as sheldonross does it.

    Leave a comment:


  • sheldonross
    replied
    I just spray, cure,spray cure,spray cure... never had any problems so far

    Leave a comment:


  • tavo1765
    started a topic 3 coat process

    3 coat process

    What are some of the ways you guys do 3 stage coatings?


    -Do you for example lets say use a chrome base, go half cure, add a clear with flakes do a half cure, and finish with a candy top coat for a full cure cycle or??

    -chrome base again, half cure. Then add a candy and want to make it look more deeper and add a high gloss clear would you only have to go partial cures on the chrome/candy then full on the clear

    Or can I just go and fully cure the chrome then apply a candy to a half cure and add a clear on top and go full cure..