What are some of the ways you guys do 3 stage coatings?
-Do you for example lets say use a chrome base, go half cure, add a clear with flakes do a half cure, and finish with a candy top coat for a full cure cycle or??
-chrome base again, half cure. Then add a candy and want to make it look more deeper and add a high gloss clear would you only have to go partial cures on the chrome/candy then full on the clear
Or can I just go and fully cure the chrome then apply a candy to a half cure and add a clear on top and go full cure..


-Do you for example lets say use a chrome base, go half cure, add a clear with flakes do a half cure, and finish with a candy top coat for a full cure cycle or??
-chrome base again, half cure. Then add a candy and want to make it look more deeper and add a high gloss clear would you only have to go partial cures on the chrome/candy then full on the clear
Or can I just go and fully cure the chrome then apply a candy to a half cure and add a clear on top and go full cure..