I posted some new pictures of my oven. It's 8' x8' electric. It runs on 8 -3100w heating elements. 2 - Thermostats controlled by 2 - 50 amp relays. It comes up to 400F in 15 minutes. Once over 350F, 4 of the 8 elements shut down & it stays at 400F with just 4 elements running.
I would have posted more pic's, but the album bumped them stating "pictures are too large or file is corupted"?? I made sure they were smaller than the 800 x 600 pixels??
Bob
I would have posted more pic's, but the album bumped them stating "pictures are too large or file is corupted"?? I made sure they were smaller than the 800 x 600 pixels??
Bob