    why i was doing my upper a arms i sprayed white baked it let the part get too 120 130 or so then went over it with tropical orange and got tropical poo it looked like when u put put paint stripper on something before u strip it on the one side and i put a good coating on and it still didnt look like it covered evenly and how do u prep the peice for recoating thanx

  • #2
    you can put the part in a oven and set it at clean 800F this should aid in the removal by baking it off. to prep after coated . I use a sharp oxide ot steel to remove it. it is best to remove if you have alot of defects in the coating .

    Good luck. and happy powdering :'