    Has anyone sprayed ceramic over chrome?.. and if so, what was your prep process...?
    If it jams; Force it. And if it breaks it needed replacing anyway.

    I can go from 0 to "What seems to be the problem Officer?" in 3 seconds."

  • #2
    Will not work the way you want it ... you need to do 2 thing's either blast the chrome off or have the part steel shot then blast with oxide.. to get the ceramic to stick

    Comment


    • #3
      thanks for the info!!