    Anyone used the Cerakote or Chromex high temp ceramic coatings Caswell sells here, and what were the results?

    I realize it requires an HVLP sprayer and not Powder Gun, but it seems to be in the powder section of the website, so I thought I'd post here first.

    Thanks

    Keith

  • #2
    Never used them, but it sounds interesting... I too am curious to hear from some people who have used them.

    Comment


    • #3
      I use chromex a lot , once polish it looks as close to chrome as you can get.
      they are not powder coatings they are liquid paints and require to bake at 500 for 1 hour

      techlines coatings are also geat
      both will stand very high temperatures with out dulling or peeling off