I use chromex a lot , once polish it looks as close to chrome as you can get.
they are not powder coatings they are liquid paints and require to bake at 500 for 1 hour
techlines coatings are also geat
both will stand very high temperatures with out dulling or peeling off
there are pictures of the coatings on the album at the top.
Announcement
Collapse
No announcement yet.
High temp coatings
Collapse
X
-
Never used them, but it sounds interesting... I too am curious to hear from some people who have used them.
Leave a comment:
-
High temp coatings
Anyone used the Cerakote or Chromex high temp ceramic coatings Caswell sells here, and what were the results?
I realize it requires an HVLP sprayer and not Powder Gun, but it seems to be in the powder section of the website, so I thought I'd post here first.
Thanks
KeithTags: None
Leave a comment: