will powder coating work on shock springs, the flexing

Collapse
X
 
  • Filter
  • Time
  • Show
Clear All
new posts

  • trsick
    replied
    Re: will powder coating work on shock springs, the flexing

    Go for it Corey:
    I have done a ton of springs, in fact I have a set on display in my store front, it helps sell the powder. People pick it up & bend it all around & can see for themselves how well the powder holds & how flexable it is.
    Good Luck
    Bob

    Leave a comment:


  • corybarta
    replied
    thanks for the info

    Leave a comment:


  • CaptainChauncy
    replied
    It should hold up fine, I have powdercoated lots of atv springs and never had a problem

    Leave a comment:


  • will powder coating work on shock springs, the flexing

    I want to powder coat my shock springs on my snowmobile, will it hold up to the constant flexing.