    I'm looking for information as to which chrome is the better of the two "super" or "near"? I have a chrome from another company and mostly it looks like silver paint or that cheap "chrome spray" paint. Also looking for tips on prepping for chrome, and cool down/preheat process for chrome and clear. All the other colors I've tried have worked good so far, the chrome just keeps messin up on me
    Save the trees- burn Rubber!
    };^)>

  • #2
    super is the better of the two, I found that it works and looks better on smaller parts like brackets, start doing large flat areas and it looks like really good silver paint.
    Pro-Tech Powder Coating
    93976 Ocean Way
    541-247-8168
    [email protected]
    Gold Beach,Oregon

    Comment


    • #3
      yeah I was doin a door for a side tool box and not to impressed with the outcome. also I can't sem to get rid of orange peel any help?
      Save the trees- burn Rubber!
      };^)>

      Comment


      • #4
        orange peel can be caused by over build or the gun to close to the part wich most of the time leads to over build.

        Comment


        • #5
          Cant you get the same results coating over white with candy instead of coating over chrome?

          Comment


          • #6
            yes but usually the part will come out darker..