  • Tape over powder.....

    OK heres my situation;
    i need to do multiple colors on a part... once my base color is down, will the tape screw up the cured base by curing the 2nd and 3rd colors
    If it jams; Force it. And if it breaks it needed replacing anyway.

    I can go from 0 to "What seems to be the problem Officer?" in 3 seconds."

  • #2
    it's easier said than done
    you have to fully cure each coat and let cool down completely
    or otherwise it will mark the taped previous coat.
    I suggest to practice on some scrap pieces first to get the hang of it .

    Comment


    • #3
      Thanks for the tip jtagger, ill give it a try.